জিআই ফাঁপা পাইপের আকার
| আরএইচএস ডিএক্সবি মিমি | সেকেন্ড এলাকা A সেমি2 | পুরু। মিমি | একক W Kg/m | চক্রগতির ব্যাসার্ধ | নিষ্ক্রিয়তা মুহূর্ত | টরসিয়নাল কনস্ট্যান্টস | ইলাস্টিক মডুলাস | বাইরের পৃষ্ঠ | ||||
| ryyসেমি | rxxসেমি | Iyyসেমি4 | Ixxসেমি4 | জে সেমি4 | খ সেমি3 | Zyyসেমি3 | Zxxসেমি3 | ক্ষেত্রফল প্রতি মিমি2 | ||||
| 50x25 | 2.74 | 2.00 | 2.15 | 10.10 | 1.75 | 2.81 | 8.38 | 6.79 | 3.79 | 2.25 | 3.35 | 0.142 |
| 3.46 | 2.60 | 2.71 | 0.99 | 1.71 | 3.36 | 10.16 | 8.27 | 4.53 | 2.69 | 4.06 | 0.137 | |
| 4.13 | 3.20 | 3.24 | 0.96 | 1.68 | 3.80 | 11.63 | 9.52 | 5.12 | 3.04 | 4.65 | 0.134 | |
| 4.95 | 4.00 | 3.88 | 0.92 | 1.63 | 4.23 | 13.13 | 10.86 | 5.69 | 3.38 | 5.25 | 0.129 | |
| 60x40 | 4.76 | 2.60 | 3.73 | 1.59 | 2.19 | 12.09 | 22.76 | 25.59 | 9.83 | 6.05 | 7.59 | 0.187 |
| 5.25 | 2.90 | 4.12 | 1.58 | 2.17 | 13.11 | 24.74 | 28.02 | 10.66 | 6.56 | 8.25 | 0.185 | |
| 6.35 | 3.60 | 4.98 | 1.55 | 2.13 | 15.23 | 28.90 | 33.30 | 12.41 | 7.62 | 9.63 | 0.181 | |
| 7.67 | 4.50 | 6.02 | 1.51 | 2.08 | 17.44 | 33.31 | 39.34 | 14.29 | 8.72 | 11.10 | 0.177 | |
| 66x33 | 4.70 | 2.60 | 3.69 | 1.34 | 2.31 | 8.43 | 25.15 | 20.75 | 8.71 | 5.11 | 7.62 | 0.185 |
| 5.19 | 2.90 | 4.07 | 1.33 | 2.29 | 9.12 | 27.33 | 22.65 | 9.43 | 5.53 | 8.28 | 0.183 | |
| 6.28 | 3.60 | 4.93 | 1.29 | 2.25 | 10.52 | 31.87 | 26.71 | 10.90 | 6.37 | 9.66 | 0.179 | |
| 7.58 | 4.50 | 5.95 | 1.25 | 2.20 | 11.93 | 36.64 | 31.21 | 12.43 | 7.23 | 11.10 | 0.175 | |
| 80x40 | 5.80 | 2.60 | 4.55 | 1.65 | 2.84 | 15.74 | 46.58 | 38.50 | 13.46 | 7.87 | 11.65 | 0.227 |
| 7.01 | 3.20 | 5.50 | 1.62 | 2.80 | 18.41 | 54.94 | 45.83 | 15.78 | 9.21 | 13.74 | 0.224 | |
| 8.55 | 4.00 | 6.71 | 1.59 | 2.75 | 21.49 | 64.79 | 54.77 | 18.49 | 10.74 | 16.20 | 0.219 | |
| 10.01 | 4.80 | 7.85 | 1.55 | 2.71 | 24.03 | 73.22 | 62.81 | 20.79 | 12.02 | 18.30 | 0.215 | |
| 96x48 | 8.54 | 3.20 | 6.71 | 1.97 | 3.40 | 33.28 | 98.61 | 82.13 | 23.82 | 13.87 | 20.54 | 0.272 |
| 10.47 | 4.00 | 8.22 | 1.94 | 3.35 | 39.32 | 117.54 | 99.11 | 28.24 | 16.38 | 24.49 | 0.267 | |
| 12.31 | 4.80 | 9.66 | 1.90 | 3.30 | 44.55 | 134.35 | 114.80 | 32.14 | 18.56 | 27.99 | 0.263 | |
| 122x61 | 12.32 | 3.60 | 9.67 | 2.53 | 4.34 | 78.83 | 232.61 | 193.91 | 44.50 | 25.84 | 38.13 | 0.347 |
| 15.14 | 4.50 | 11.88 | 2.49 | 4.29 | 93.78 | 278.94 | 235.39 | 53.13 | 30.75 | 45.73 | 0.343 | |
| 17.85 | 5.40 | 14.01 | 2.45 | 4.24 | 107.03 | 320.83 | 274.29 | 60.89 | 35.09 | 52.60 | 0.338 | |
| 145x82 | 20.28 | 4.80 | 15.92 | 3.36 | 5.23 | 228.50 | 555.16 | 534.27 | 94.45 | 55.73 | 76.57 | 0.429 |
| 22.60 | 5.40 | 17.74 | 3.33 | 5.20 | 250.59 | 610.85 | 592.70 | 103.81 | 61.12 | 84.26 | 0.426 | |
| 172x92 | 23.83 | 4.80 | 18.71 | 3.82 | 6.20 | 346.91 | 917.13 | 826.04 | 128.85 | 75.41 | 106.64 | 0.503 |
| 26.59 | 5.40 | 20.88 | 3.79 | 6.17 | 381.74 | 1012.47 | 918.10 | 142.04 | 82.99 | 117.73 | 0.500 | |
| 200x100 | 22.95 | 4.00 | 18.01 | 4.23 | 7.23 | 410.78 | 1199.71 | 991.47 | 141.46 | 82.16 | 119.97 | 0.579 |
| 28.36 | 5.00 | 22.26 | 4.19 | 7.17 | 496.94 | 1459.25 | 1216.96 | 171.53 | 99.39 | 145.93 | 0.574 | |
| 33.63 | 6.00 | 26.40 | 4.14 | 7.12 | 576.91 | 1703.31 | 1434.03 | 199.68 | 115.38 | 170.33 | 0.569 | |
| 43.79 | 8.00 | 34.38 | 4.05 | 7.00 | 719.19 | 2146.21 | 1843.86 | 250.68 | 143.84 | 214.62 | 0.559 | |
| 240x120 | 27.75 | 4.00 | 21.78 | 5.11 | 8.72 | 725.35 | 2110.72 | 1736.39 | 208.03 | 120.29 | 175.89 | 0.699 |
| 34.36 | 5.00 | 26.97 | 5.07 | 8.67 | 882.47 | 2579.67 | 2138.48 | 253.55 | 147.08 | 214.97 | 0.694 | |
| 40.83 | 6.00 | 32.05 | 5.02 | 8.61 | 1030.45 | 3025.91 | 2528.39 | 296.70 | 171.74 | 252.16 | 0.689 | |
| 53.39 | 8.00 | 41.91 | 4.93 | 8.49 | 1299.95 | 3851.84 | 3272.90 | 376.29 | 216.66 | 320.99 | 0.679 | |
| 300x150 | 51.63 | 6.00 | 40.53 | 6.35 | 10.85 | 2079.57 | 6073.51 | 5034.64 | 478.20 | 277.28 | 404.90 | 0.869 |
| 67.79 | 8.00 | 53.22 | 6.26 | 10.73 | 2654.12 | 7807.95 | 6559.05 | 612.64 | 353.88 | 520.53 | 0.859 | |
| 83.43 | 10.00 | 65.49 | 6.17 | 10.62 | 3173.71 | 9403.90 | 8011.67 | 736.01 | 423.16 | 626.93 | 0.848 | |
| 300x200 | 57.63 | 6.00 | 45.24 | 8.29 | 11.31 | 3962.19 | 7370.23 | 8186.02 | 650.85 | 296.22 | 491.35 | 0.969 |
| 75.79 | 8.00 | 59.50 | 8.20 | 11.12 | 5097.04 | 9513.66 | 10722.83 | 839.51 | 509.70 | 634.24 | 0.959 | |
| 93.43 | 10.00 | 73.34 | 8.11 | 11.10 | 6144.30 | 11507.24 | 13169.70 | 1015.43 | 614.43 | 767.15 | 0.948 | |